Nickel Alloy 200 Solid Steel Round Bar
Nickel 200 is a 99.6% pure nickel alloy that is one of the toughest metals in existence. It has excellent mechanical properties and high thermal and electrical conductivity. Additionally, the beneficial properties of Nickel 200 and its chemical composition make it easy to manufacture and highly resistant to corrosive environments.
Nickel 200 is commonly used in the manufacture of components in aerospace equipment such as turbine blades, combustors, nozzles and propulsion systems. Nickel 200 is widely used in the aerospace industry due to its corrosion resistance and high temperature stability.
nickel alloy 200 round bar sizes
| 3.00 – 75.00 | 1/8" – 3.00" | h8-h9-h10-h11, ASTM B160 | |
| 10.00 – 75.00 | 5/6" – 2.50" | h8-h9-h10-h11 | |
| 40.00 – 150.00 | 1.50" – 6.00" | h11, ASTMA-484 h11-DIN 1013 | |
| 20.00 – 50.00 | 3/4″ – 2.00" | h9-h10-h11, ASTM B160 |
nickel 200 Alloy Steel Round Bar chemical composition
| C | S | ||||||||
|---|---|---|---|---|---|---|---|---|---|
| Nickel 200 | 99.0 min | 0.4 max | 0.15 max | 0.35 max | 0.1 max | 0.25 max | - | - | 0.01 max |
nickel 200 Alloy Steel Rods mechanical property
| Nickel Alloy 200 Round Bars Mechanical Properties: |
| Yield Strength (0.2%Offset) | ||||
|---|---|---|---|---|
| 8.9 g/cm3 | 1446 ℃ (2635 ℃F) | Psi – 67000 , MPa – 462 | Psi – 21500 , MPa – 148 | 45 % |
Equipment applications of nickel 200 in corrosive environments
In corrosive environments, Nickel 200 is often used to manufacture corrosion-resistant equipment, such as chemical equipment, reactors, storage tanks, pipes and valves. Because nickel 200 has excellent corrosion resistance, it can resist corrosion from corrosive media such as acids, alkalis, and salts, and can maintain stability and performance in harsh chemical environments. This makes Nickel 200 the material of choice in many industrial sectors, especially for equipment requiring high corrosion resistance.



We have enough weathering steel in stock, and we can also customize it according to your needs.
Populárne Tagy: nickel alloy 200 solid steel round bar, China nickel alloy 200 solid steel round bar manufacturers, suppliers, factory, Zliatiny nikluC7701 Copper nikel zliatiny Round ROOD