Žehlička s rovnakým uhlom
Rovnaké uhly okrajov majú dve rovnaké šírky okrajov. Jeho špecifikácie sú vyjadrené ako počet milimetrov šírky strany × šírka strany × hrúbka strany. Ako napríklad "∟30x30x3", to znamená šírka strany 30 mm, hrúbka strany 3 mm rovnostranný uhol. Dá sa vyjadriť aj v modeli, model je počet centimetrov šírky strany, napríklad ∟3 #.
rovnaké rozmery uhlových tyčí
| Veľkosť (v x in) |
Rozmery | Statické parametre | |||
|---|---|---|---|---|---|
| Hĺbka - h - (v) |
Hrúbka - s - (v) |
Sekčná oblasť (v2) |
Hmotnosť (lbf/ft) |
Moment zotrvačnosti - Ix - (v4) |
|
| 12 x 12 | 12 | 1 3/8 | 30.9 | 105 | 410.0 |
| 12 | 1 1/4 | 28.3 | 96.4 | 377.5 | |
| 12 | 1 1/8 | 25.6 | 87.2 | 344.1 | |
| 12 | 1 | 22.9 | 77.8 | 310.4 | |
| 10 x 10 | 10 | 1 3/8 | 25.6 | 87.1 | 232.1 |
| 10 | 1 1/4 | 23.5 | 79.9 | 215.1 | |
| 10 | 1 1/8 | 21.2 | 72.3 | 196.2 | |
| 10 | 1 | 19.0 | 64.7 | 177.3 | |
| 10 | 7/8 | 16.7 | 56.9 | 157.6 | |
| 10 | 3/4 | 14.4 | 49.1 | 137.2 | |
| 8 x 8 | 8 | 1 1/8 | 16.7 | 56.9 | 98.0 |
| 8 | 1 | 15.0 | 51.0 | 89.0 | |
| 8 | 7/8 | 13.2 | 45.0 | 79.6 | |
| 8 | 3/4 | 11.4 | 38.9 | 69.7 | |
| 8 | 5/8 | 9.6 | 32.7 | 59.4 | |
| 8 | 9/16 | 8.7 | 29.6 | 54.1 | |
| 8 | 1/2 | 7.8 | 26.4 | 48.6 | |
| 6 x 6 | 6 | 1 | 11.0 | 37.4 | 35.5 |
| 6 | 7/8 | 9.7 | 33.1 | 31.9 | |
| 6 | 3/4 | 8.4 | 28.7 | 28.2 | |
| 6 | 5/8 | 7.1 | 24.2 | 24.2 | |
| 6 | 9/16 | 6.4 | 21.9 | 22.1 | |
| 6 | 1/2 | 5.8 | 19.6 | 19.9 | |
| 6 | 7/16 | 5.1 | 17.2 | 17.7 | |
| 6 | 3/8 | 4.4 | 14.9 | 15.4 | |
| 6 | 5/16 | 3.7 | 12.4 | 13.0 | |
| 5 x 5 | 5 | 7/8 | 8.0 | 27.2 | 17.8 |
| 5 | 3/4 | 6.9 | 23.6 | 15.7 | |
| 5 | 5/8 | 5.9 | 20.0 | 13.6 | |
| 5 | 1/2 | 4.8 | 16.2 | 11.3 | |
| 5 | 7/16 | 4.2 | 14.3 | 10.0 | |
| 5 | 3/8 | 3.6 | 12.3 | 8.74 | |
| 5 | 5/16 | 3.0 | 10.3 | 7.42 | |
| 4 x 4 | 4 | 3/4 | 5.4 | 18.5 | 7.67 |
| 4 | 5/8 | 4.6 | 15.7 | 6.66 | |
| 4 | 1/2 | 3.8 | 12.8 | 5.56 | |
| 4 | 7/16 | 3.3 | 11.3 | 4.97 | |
| 4 | 3/8 | 2.9 | 9.8 | 4.36 | |
| 4 | 5/16 | 2.4 | 8.2 | 3.71 | |
| 4 | 1/4 | 1.9 | 6.6 | 3.04 | |
| 3 1/2 x 3 1/2 | 3 1/2 | 1/2 | 3.3 | 11.1 | 3.64 |
| 3 1/2 | 7/16 | 2.9 | 9.8 | 3.26 | |
| 3 1/2 | 3/8 | 2.5 | 8.5 | 2.87 | |
| 3 1/2 | 5/16 | 2.1 | 7.2 | 2.45 | |
| 3 1/2 | 1/4 | 1.7 | 5.8 | 2.01 | |
| 3 x 3 | 3 | 1/2 | 2.75 | 9.4 | 2.22 |
| 3 | 7/16 | 2.43 | 8.3 | 1.99 | |
| 3 | 3/8 | 2.11 | 7.2 | 1.76 | |
| 3 | 5/16 | 1.78 | 6.1 | 1.51 | |
| 3 | 1/4 | 1.44 | 4.9 | 1.24 | |
| 3 | 3/16 | 1.09 | 3.7 | 0.96 | |
| 2 1/2 x 2 1/2 | 2 1/2 | 1/2 | 2.25 | 7.7 | 1.23 |
| 2 1/2 | 3/8 | 1.73 | 5.9 | 0.98 | |
| 2 1/2 | 5/16 | 1.46 | 5.0 | 0.85 | |
| 2 1/2 | 1/4 | 1.19 | 4.1 | 0.70 | |
| 2 1/2 | 3/16 | 0.90 | 3.1 | 0.55 | |
| 2 x 2 | 2 | 3/8 | 1.36 | 4.7 | 0.48 |
| 2 | 5/16 | 1.15 | 3.9 | 0.42 | |
| 2 | 1/4 | 0.94 | 3.2 | 0.35 | |
| 2 | 3/16 | 0.72 | 2.4 | 0.27 | |
| 2 | 1/8 | 0.48 | 1.7 | 0.19 | |
rovný oceľový uholník Product image

Fotografia skupiny GNEE

Návšteva zákazníka skupiny GNEE

Skupina GNEE sa zúčastňuje zahraničných výstav ocele

Máme profesionálny personál, ktorý vám poskytne podrobné odpovede na vaše objednávky. Ak máte akékoľvek otázky týkajúce sa žehličky s rovnakým uhlom, kontaktujte ma.
Populárne Tagy: železo s rovnakým uhlom, Čína výrobcovia s rovnakým uhlom železa, dodávatelia, továreň, Uhlová oceľ