P355GH and S355J2 (often grouped with P355J2) are high-strength, weldable steels, but differ in application: P355GH (EN 10028-2) is a pressure vessel steel designed for elevated temperatures, used in boilers and petrochemicals, with good plasticity and weldability. S355J2 (EN 10025-2) is a structural steel known for good strength and low-temperature toughness (down to -20℃), ideal for general construction, bridges, and cold regions, featuring good weldability and impact resistance. Both offer excellent strength (around 355 MPa yield), but their 'G' (heat-resistant) vs 'J2' (low-temp impact) designations define their primary uses.
P355GH (Pressure Vessel)
Standard: EN 10028-2
Key Feature: Designed for high-temperature service (e.g., in boilers, steam drums).
Properties: Good plasticity, toughness, cold bending, and welding performance.
Applications: Boilers, pressure vessels, petrochemical equipment.
S355J2 (Structural)
Standard: EN 10025-2 (Note: often referenced as S355J2)
Key Feature: Excellent low-temperature impact toughness (Charpy-V test at -20℃).
Properties: Medium tensile strength, readily weldable, good general toughness.
Applications: Construction, bridges, cold-region projects, general engineering.
Temperature: P355GH excels in hot conditions; S355J2 excels in cold conditions.
Standard: Different European standards (EN 10028-2 vs. EN 10025-2).
Primary Use: P355GH for pressure/heat; S355J2 for general structure/cold.
|
P355GH Chemical Composition |
|||||||
|
C |
P |
S |
N |
||||
|
P355GH |
0.10-0.22 |
0.60 |
1.10-1.70 |
0.025 |
0.015 |
0.020 |
0.012 |
|
V |
|||||||
|
0.30 |
0.30 |
0.08 |
0.040 |
0.30 |
0.03 |
0.02 |
|
S355J2 Chemical composition
|
C |
|
|
|
P |
S |
|
|
|
max 0.24 |
0.60 |
1.70 |
|
Max 0.035 |
Max 0.035 |
|
|
|
V |
|
|
N |
|
|
|
|
|
|
|
|
|
0.60 |
|
|
|
P355GH Mechanical Property
|
|
P355GH Mechanical Property |
||||||
|
P355GH |
-20℃ |
0℃ |
+20℃ |
||||
|
<= 16 |
355 |
510-650 |
20 |
27 |
34 |
40 |
|
|
16> to <=40 |
345 |
510-650 |
20 |
27 |
34 |
40 |
|
|
40> to <=60 |
335 |
510-650 |
20 |
27 |
34 |
40 |
|
|
60> to <=100 |
315 |
490-630 |
20 |
27 |
34 |
40 |
|
|
100> to <=150 |
295 |
480-630 |
20 |
27 |
34 |
40 |
|
|
150> to <=250 |
280 |
470-630 |
20 |
27 |
34 |
40 |
|
S355J2 Mechanical Property
|
|
-150 |
150-250 |
250-400 |
|
|||||||||||
|
Temperature(-20) |
27 |
27 |
27 |
|
|||||||||||
|
|
to 16 |
16 - 40 |
40 - 63 |
63 - 80 |
80 - 100 |
100 - 150 |
150 - 200 |
200-250 |
250-400 |
||||||
|
ReH - Minimum yield strength (MPa) |
355 |
345 |
335 |
325 |
315 |
295 |
285 |
275 |
265 |
||||||
|
|
-3 |
3-100 |
100-150 |
150-250 |
250-400 |
||||||||||
|
Rm -Tensile strength (MPa) |
510-680 |
470-630 |
450-600 |
450-600 |
450-600 |
||||||||||
|
|
3-40 |
40-63 |
63-100 |
100-150 |
150-250 |
250-400 |
|
A - Minimum elongation Lo=5,65 √ So (%) |
22 |
21 |
20 |
18 |
17 |
17 |