S355J2WP steel plate

Nov 19, 2025 Zanechajte správu

S355J2WP steel grade is a hot rolled products of structural steels in technical delivery conditions with improved atmospheric corrosion resistance.The main alloying elements are chromium nickel and copper with added phosphorous which gives it excellent self protecting qualities. As the steel reacts with elements in the atmosphere, the material forms a layer of rust over time which in essence protects the steel from corrosion.

 

Chemical composition % of the Product analysis of grade S355J2WP

 

C

P

S

N

0.15

0.80

1.10

0.20-0.60

0.05-0.16

0.035

0.25-1.35

0.010

 

Mechanical properties of grade S355J2WP

 

-20

-10

0

20

Notch impact test. Min. absorbed energy J

27

     

 

to 16

16 - 40

40 - 63

63 - 80

80 - 100

100 - 150

ReH - Minimum yield strength (MPa)

355

345

       

 

to 3

3 - 100

100-150

Rm -Tensile strength (MPa)

510-680

470-630

 

 

>=1.5<2

>=2﹤2.5

>=2.5<3

>=3<40

>=40﹤63

>=6﹤100

>=100﹤150

A - Minimum elongation Lo=5,65 √ So (%) Longitudinal

16

17

18

22